We use it in the power generating field, the stuff is unbelievably strong and can be machined if need be. we mainly use the ceramic, stainless and aluminum epoxy. this is the best stuff out there for our applications, let it cure at about 80 to 90 deg. for at least 24 hrs up to 36 hrs if you can, and your good to go! this stuff is expensive but more than worth it.